Thermal Properties Metric English Comments
Flame Spread 27.9 mm/min
1.10 in/min
ASTM D635
DuPont™ Surlyn® 9970 Ionomer Resin, Zinc  (discontinued **)
Surlyn® 9970 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr..
Flame Spread 28.0 mm/min

@Thickness 3.17 mm
1.10 in/min

@Thickness 0.125 in
FH3
LG Chemical 15NFE GPPS
High flow, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Superio..
Flame Spread 28.0 mm/min

@Thickness 3.17 mm
1.10 in/min

@Thickness 0.125 in
FH3
LG Chemical MI-730 MIPS
Flame Spread 28.0 mm/min

@Thickness 3.17 mm
1.10 in/min

@Thickness 0.125 in
FH3
LG Chemical MI-750 MIPS
Medium impact
Flame Spread 28.0 mm/min

@Thickness 3.17 mm
1.10 in/min

@Thickness 0.125 in
FH3
LG Chemical MI-770 MIPS
Flame Spread 27.9 mm/min
1.10 in/min
FM VSS-302
Multibase Multi-Flex® D 3204 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P..
Flame Spread 28.0 mm/min

@Thickness 3.17 mm
1.10 in/min

@Thickness 0.125 in
FH3
LG Chemical 60HR HIPS
Heat resistance, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include TV sets, tape recorders, vacu..
Flame Spread 27.9 mm/min
1.10 in/min
ASTM D635
DuPont™ Surlyn® 9950 Ionomer Resin, Zinc
Surlyn® 9950 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr..
Flame Spread 28.0 mm/min

@Thickness 3.17 mm
1.10 in/min

@Thickness 0.125 in
FH3
LG Chemical 15NFI GPPS