Polymer Property : Flame Spread = 1.46 in/min Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flame Spread 37.0 - 54.0 mm/min
1.46 - 2.13 in/min
Average value: 45.2 mm/min Grade Count:15
Overview of materials for Styrenic Elastomer (TES)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro..