Polymer Property : Flame Spread = 1.9 in/min Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flame Spread 47 mm/min
1.9 in/min
1.0 mm thickness; ISO 3795
Lavergne VYPET VNT 340 PET 40% Glass - Mineral Reinforced
Vypet VNT 340 is a 40% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications, with High Dielectric StrengthFeatures: High temperature performanc..
Flame Spread 47 mm/min
1.9 in/min
burn rate
AlphaGary Evoprene™ GF 6256 Automotive Thermoplastic Elastomer
Evoprene™ GF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab..