Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 55 mm/min @Thickness 2.00 mm |
2.2 in/min @Thickness 0.0787 in |
US-FMVSS; ISO 3795 |
Ineos ABS Lustran® ABS E211 LNS013 Pellets (a-methylstyrene-SAN-modified), Extrusion Grade Lustran® ABS E211 LNS013 is extrusion grade with high heat resistance. It is used for the production of molded plastic articles. |
|||
Flame Spread | 55 mm/min @Thickness 2.00 mm |
2.2 in/min @Thickness 0.0787 in |
US-FMVSS; ISO 3795 |
Styrolution Novodur® P2M-AT ABS Pellets Novodur® P2M-AT has high impact strength, high gloss, and contains antistatic additive. It is used for the production of molded plastic articles. |
|||
Flame Spread | 55 mm/min @Thickness 2.00 mm |
2.2 in/min @Thickness 0.0787 in |
US-FMVSS; ISO 3795 |
Styrolution Novodur® P2M-V ABS Pellets Novodur® P2M-V has high impact strength, high gloss, and low emission. It is used for the production of molded plastic articles. |
|||
Flame Spread | 55 mm/min | 2.2 in/min | Horizontal Burning Speed 2mm thickness; ISO 3795 |
Styron Magnumâ„¢ 3453 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3453 ABS is a general purpose injection molding resin suitable for a wide range of applications.Information provided by DowThis product line was spun off from Dow Chemical to Styron in .. |
|||
Flame Spread | 55 mm/min @Thickness 1.00 mm |
2.2 in/min @Thickness 0.0394 in |
ISO 3795 (FMVSS 302) |
DuPont Performance Polymers Delrin® 500T BK602 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer Delrin 500T BK602 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri.. |
|||
Flame Spread | 55 mm/min @Thickness 1.00 mm |
2.2 in/min @Thickness 0.0394 in |
ISO 3795 (FMVSS 302) |
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 6 Minlon 73GM40 NC010 is a 40% mineral/glass reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Poly.. |