Thermal Properties Metric English Comments
Flame Spread 55.9 mm/min
2.20 in/min
FVSS302/SAE J369 in/min
Kraton® G7820 GU-N (SEBS) Compound
Description: Kraton G7820 GU-N is an easy processing, general purpose 90 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..