Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 43 mm/min | 1.7 in/min | burn rate |
AlphaGary Evoprene™ GF 6257 Automotive Thermoplastic Elastomer Evoprene™ GF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Flame Spread | 43 mm/min | 1.7 in/min | burn rate |
AlphaGary Evoprene™ LF 6151 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |