Polymer Property : Flame Spread = 53 mm/min Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flame Spread 53 mm/min

@Thickness 1.00 mm
2.1 in/min

@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
DuPont Performance Polymers Delrin® 570 NC000 Acetal (POM)  (Unverified Data**)
20% Glass Filled Medium Viscosity Acetal Homopolymer Delrin 570 NC000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler for injection molding. Delrin 570 has very high stiff..