Polymer Property : Flame Spread = 7.6 mm/min Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flame Spread <= 7.6 mm/min
<= 0.30 in/min
Burning Rate UL 94 HB; ASTM D635
Spartech Polycast Poly FR9 (0.060") Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flame Spread 7.6 mm/min
0.30 in/min
VSS-302
Multibase Multi-Flex® A 6202 MR TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..