Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | -0.700 - -0.300 µm/m-°C @Temperature 20.0 °C |
-0.389 - -0.167 µin/in-°F @Temperature 68.0 °F |
Longitudinal |
Goodfellow Carbon/Epoxy Composite Rod Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow. |