Thermal Properties Metric English Comments
CTE, linear -0.300 - 0.300 µm/m-°C

@Temperature 20.0 - 700 °C
-0.167 - 0.167 µin/in-°F

@Temperature 68.0 - 1290 °F
Schott ROBAX® Glass Ceramic
ROBAX® is a highly transparent glass-ceramic having virtually zero thermal expansion and sufficient mechanical resistance required for all standard applications. It is produced in flat, rolled s..
CTE, linear -0.300 - 0.500 µm/m-°C

@Temperature 20.0 - 100 °C
-0.167 - 0.278 µin/in-°F

@Temperature 68.0 - 212 °F
Reade Advanced Materials Petalite Powder (Li2O·Al2O3·8SiO2)
Description: Rare, light and fragile with tabular or columnar crystals. A monoclinic mineral with a framework silicate structure. Its color is creamy to white and sometimes to more rarely pinkish. I..