Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 0.600 µm/m-°C @Temperature 30.0 - 300 °C |
0.333 µin/in-°F @Temperature 86.0 - 572 °F |
|
Mo-Sci Corporation GL-0201 Silica Glass Spheres Appearance: Solid clear amorphous silica microspheres with white color in powder form.Typical applications of GL0201 beads include: calibration, high temperature spacer material for gauge control, c.. |
|||
CTE, linear | 0.600 µm/m-°C @Temperature 20.0 °C |
0.333 µin/in-°F @Temperature 68.0 °F |
|
Ceradyne Thermo-Sil® HS Fused Silica Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi.. |
|||
CTE, linear | 0.600 µm/m-°C @Temperature 20.0 °C |
0.333 µin/in-°F @Temperature 68.0 °F |
|
Ceradyne Thermo-Sil® Isomolded™ Fused Silica Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi.. |