Thermal Properties Metric English Comments
CTE, linear 0.504 - 0.774 µm/m-°C
0.280 - 0.430 µin/in-°F
Average value: 0.583 µm/m-°C Grade Count:5
Overview of materials for Ethylene Butyl Acrylate
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp..