CTE, linear 1.30 µm/m-°C

@Temperature 20.0 - 300 °C
0.722 µin/in-°F

@Temperature 68.0 - 572 °F
ISO 7991
Schott Glass 8228 Intermediate sealing glass
Used for sealing to Quartz Glass and Glass 8229 The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by SCHOTT AG.