Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 1.56 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 2.80 - 70.0 µm/m-°C
1.56 - 38.9 µin/in-°F
Average value: 49.4 µm/m-°C Grade Count:7
Overview of materials for Cyclo Olefin Polymer
This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria..
CTE, linear 2.80 µm/m-°C

@Temperature 260 °C
1.56 µin/in-°F

@Temperature 500 °F
Ferro EG 1001 Metal Sealing
Glass Type: Si-B Typical Powder Form: VSD Typical Application: Gun Mount Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals for..
CTE, linear 2.80 µm/m-°C

@Temperature 20.0 - 100 °C
1.56 µin/in-°F

@Temperature 68.0 - 212 °F
UCAR Carbon UCAR® ATA Isostatic Molded Graphite
Economical grade ATA is the lowest density version of isostatically molded, fine grain grade ATJ family of graphite materials.Typical Applications: ATA is used in general purpose applications where ..
CTE, linear 2.80 µm/m-°C

@Temperature 20.0 - 100 °C
1.56 µin/in-°F

@Temperature 68.0 - 212 °F
UCAR Carbon UCAR® ATJ Isostatic Molded Graphite
Isostatically molded ATJ has been an industry standard for many years. It is a fine grain, high strength material which can be machined to precise tolerances and a fine surface finish. Grade ATJ has..
CTE, linear 2.80 µm/m-°C

@Temperature 20.0 - 100 °C
1.56 µin/in-°F

@Temperature 68.0 - 212 °F
UCAR Carbon UCAR® ATR Isostatic Molded Graphite
Isostatically molded ATR is a lower density version of grade ATJ. It is a fine grain, high strength material which can be machined to precise tolerances and a fine surface finish.Typical Application..
CTE, linear 2.80 µm/m-°C

@Temperature 0.000 - 300 °C
1.56 µin/in-°F

@Temperature 32.0 - 572 °F
Corning 7761 Potash Borosilicate Crushed/Powdered Glass
Available in mesh sizes 4 through 325 and can be customized. Used for sealing and other applications.Information provided by Corning Incorporated.
CTE, linear 2.80 µm/m-°C
1.56 µin/in-°F
Volumetric thermal expansion
China-Yixing Longly Refractories Seggar SiC
SiC series products of SiC shelf boards, SiC pillars, SiC slab, SiC seggar kiln furniture, are formed using high-quality silicon carbide materials and high temperature binders by tons of high-vibrat..
CTE, linear 2.80 µm/m-°C

@Temperature 27.0 - 175 °C
1.56 µin/in-°F

@Temperature 80.6 - 347 °F
ASTM D696
3M 7997MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
CTE, linear 2.80 µm/m-°C

@Temperature 20.0 °C
1.56 µin/in-°F

@Temperature 68.0 °F
Potters Industries Spheriglass® 3000E Solid Glass Spheres
Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage..