Polymer Property : CTE, linear = 1.70 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 1.70 µm/m-°C

@Temperature 20.0 °C
0.944 µin/in-°F

@Temperature 68.0 °F
Ceradyne Thermo-Sil® Castable 220 Fused Silica
Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi..