Polymer Property : CTE, linear = 118 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 118 µm/m-°C

@Temperature 20.0 °C
65.6 µin/in-°F

@Temperature 68.0 °F
Cytec EN-2552 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
CTE, linear 118 µm/m-°C

@Temperature 20.0 °C
65.6 µin/in-°F

@Temperature 68.0 °F
Cytec EN-2551 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..