Polymer Property : CTE, linear = 143 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 143 µm/m-°C

@Temperature 20.0 °C
79.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Lubrizol Pellethane® 2363-55D Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
CTE, linear 143 µm/m-°C
79.4 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® H31D-LV Epoxy
Material Description: A single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and optoelectronic packaging. It i..