Thermal Properties Metric English Comments
CTE, linear 260 µm/m-°C

@Temperature 20.0 °C
144 µin/in-°F

@Temperature 68.0 °F
3M Dyneon™ Fluorel™ Dipolymer, 35% Carbon Black Filled  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.66% fluorine content. See the many specific grades of Fluorel™ fluoroelastomer in MatWeb.