Thermal Properties Metric English Comments
CTE, linear 149 µm/m-°C

@Temperature 20.0 °C
82.8 µin/in-°F

@Temperature 68.0 °F
Dow Pellethane® 2102-90AR Polyurethane Elastomer, Polyester Polycaprolactone Based  (discontinued **)
PELLETHANE® 2102-90AR elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with enhanced mold release, low compression set, a..
CTE, linear 149 µm/m-°C

@Temperature 20.0 °C
82.8 µin/in-°F

@Temperature 68.0 °F
Trelleborg Emerson & Cuming Stycast® E 1400 Two-Component General Purpose Encapsulant
Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as ..