CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Strip
General Elgiloy® information: High strength, ductility, fatigue life, and good mechanical properties. Corrosion resistant in numerous environments. Available in strip (currently 0.0015" to 0.075"..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Strip, 10% Cold Reduction
The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Strip, 20% Cold Reduction
The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Strip, 20% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High ..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Strip, 30% Cold Reduction
The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Strip, 40% Cold Reduction
The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Strip, 40% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High ..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Strip, 50% Cold Reduction
The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Strip, 50% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High ..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Strip, 65% Cold Reduction
The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Strip, 65% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High ..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Strip, 85% Cold Reduction
The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Strip, 85% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High ..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Strip, Heat Treated
Heat Treatment 5 hours at 482°C. The strength and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, duc..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Wire, 10% Cold Reduction
The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Wire, 20% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Wire, 30% Cold Reduction
The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Wire, 30% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Strip, 10% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High ..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Strip, 30% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High ..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Wire, 10% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Wire, 20% Cold Reduction
The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Wire, 40% Cold Reduction
The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Wire, 40% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Wire, 47% Cold Reduction (Coil Spring Range)
45-48% cold reduction is the normal coil spring range. The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.Ge..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Wire, 47% Cold Reduction (Coil Spring Range), Heat Treated
Heat Treatment 5 hours at 527°C. 45-48% cold reduction is the normal coil spring range. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below ar..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Wire, 65% Cold Reduction
The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Wire, 65% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Wire, Heat Treated
Heat Treatment 5 hours at 527°C. The strength and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, duc..
CTE, linear 15.17 µm/m-°C

@Temperature 0.000 - 500 °C
8.428 µin/in-°F

@Temperature 32.0 - 932 °F
Elgiloy® Co-Cr-Ni Alloy, Wire
The strength and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fatigue life, and..