Polymer Property : CTE, linear = 157 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 157 µm/m-°C

@Temperature -80.0 - -30.0 °C
87.2 µin/in-°F

@Temperature -112 - -22.0 °F
ASTM D696
Lubrizol Pellethane® 2363-90A Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
CTE, linear 157 µm/m-°C
87.2 µin/in-°F
90 Minute UV Cure + Thermal; T>Tg; ASTM E831-93
3D Systems Accura® SI 40 Plastic for the SLA® 500 System
Accura 40 "Ar" or "Hc" type materials - for the SLA 500 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing ..