Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 30.4 µm/m-°C @Temperature 20.0 °C |
16.9 µin/in-°F @Temperature 68.0 °F |
|
Williams Advanced Alloys WS309 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
CTE, linear | 30.5 µm/m-°C | 16.9 µin/in-°F | |
Atom Adhesives AA-BOND 2110 Epoxy Adhesive AA-BOND 2110 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, no.. |