Polymer Property : CTE, linear = 164 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 18.0 - 164 µm/m-°C
10.0 - 91.0 µin/in-°F
Average value: 32.8 µm/m-°C Grade Count:51
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..