Thermal Properties Metric English Comments
CTE, linear 17.7 µm/m-°C

@Temperature 20.0 - 200 °C
9.83 µin/in-°F

@Temperature 68.0 - 392 °F
Materion Brush 1915â„¢ Annealed Temper Rod
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
CTE, linear 17.7 µm/m-°C

@Temperature 20.0 - 200 °C
9.83 µin/in-°F

@Temperature 68.0 - 392 °F
Materion Brush 1915â„¢ Hard Temper Rod, 0.050" - 0.375"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
CTE, linear 17.7 µm/m-°C

@Temperature 20.0 - 200 °C
9.83 µin/in-°F

@Temperature 68.0 - 392 °F
Materion Brush 1915â„¢ AT Temper Rod
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe..
CTE, linear 17.7 µm/m-°C

@Temperature 20.0 - 200 °C
9.83 µin/in-°F

@Temperature 68.0 - 392 °F
Materion Brush 1915â„¢ Hard Temper Rod, 0.375" - 0.500"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
CTE, linear 17.7 µm/m-°C

@Temperature 20.0 - 200 °C
9.83 µin/in-°F

@Temperature 68.0 - 392 °F
Materion Brush 1915â„¢ Heat Treated Temper Rod, 0.050" - 0.375"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe..
CTE, linear 17.7 µm/m-°C

@Temperature 20.0 - 200 °C
9.83 µin/in-°F

@Temperature 68.0 - 392 °F
Materion Brush 1915â„¢ Heat Treated Temper Rod, 0.375" - 0.500"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe..