Polymer Property : CTE, linear = 179.3 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 179.3 µm/m-°C

@Temperature 20.0 °C
99.61 µin/in-°F

@Temperature 68.0 °F
ASTM E-831
DSM Biomedical Elasthane™ 80A Thermoplastic Polyether Polyurethane (TPU)
A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility Elasthane™ TPU exhibits outstanding hydrolytic stabilit..