Thermal Properties Metric English Comments
CTE, linear 18.2 µm/m-°C

@Temperature 20.0 - 300 °C
10.1 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 519 Phosphor Bronzes 6%, 1/2 Hard
Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C..
CTE, linear 18.2 µm/m-°C

@Temperature 20.0 - 300 °C
10.1 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 519 Phosphor Bronzes 6%, 1/4 Hard
Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C..
CTE, linear 18.2 µm/m-°C

@Temperature 20.0 - 300 °C
10.1 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 519 Phosphor Bronzes 6%, 3/4 Hard
Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C..
CTE, linear 18.2 µm/m-°C

@Temperature 20.0 - 300 °C
10.1 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 519 Phosphor Bronzes 6%, Annealed
Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C..
CTE, linear 18.2 µm/m-°C

@Temperature 20.0 - 300 °C
10.1 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 519 Phosphor Bronzes 6%, Extra Hard
Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C..
CTE, linear 18.2 µm/m-°C

@Temperature 20.0 - 300 °C
10.1 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 519 Phosphor Bronzes 6%, Extra Spring
Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C..
CTE, linear 18.2 µm/m-°C

@Temperature 20.0 - 300 °C
10.1 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 519 Phosphor Bronzes 6%, Hard
Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C..
CTE, linear 18.2 µm/m-°C

@Temperature 20.0 - 300 °C
10.1 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 519 Phosphor Bronzes 6%, Spring
Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C..
CTE, linear 18.2 µm/m-°C

@Temperature 20.0 - 300 °C
10.1 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 521 Phosphor Bronzes 8% C, 1/2 Hard
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
CTE, linear 18.2 µm/m-°C

@Temperature 20.0 - 300 °C
10.1 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 521 Phosphor Bronzes 8% C, 1/4 Hard
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
CTE, linear 18.2 µm/m-°C

@Temperature 20.0 - 300 °C
10.1 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 521 Phosphor Bronzes 8% C, 3/4 Hard
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
CTE, linear 18.2 µm/m-°C

@Temperature 20.0 - 300 °C
10.1 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 521 Phosphor Bronzes 8% C, Annealed
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
CTE, linear 18.2 µm/m-°C

@Temperature 20.0 - 300 °C
10.1 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 521 Phosphor Bronzes 8% C, Extra Hard
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
CTE, linear 18.2 µm/m-°C

@Temperature 20.0 - 300 °C
10.1 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 521 Phosphor Bronzes 8% C, Extra Spring
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
CTE, linear 18.2 µm/m-°C

@Temperature 20.0 - 300 °C
10.1 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 521 Phosphor Bronzes 8% C, Hard
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
CTE, linear 18.2 µm/m-°C

@Temperature 20.0 - 300 °C
10.1 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 521 Phosphor Bronzes 8% C, Spring
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..