Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 18.4 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 18.4 µm/m-°C
10.2 µin/in-°F
MarkeTech Barium Fluoride, BaF2 Scintillator Crystal
Data provided by the supplier, MarkeTech International.
CTE, linear 18.4 µm/m-°C

@Temperature 20.0 - 300 °C
10.2 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 220 Commercial Bronze, 1/2 Hard
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..
CTE, linear 18.4 µm/m-°C

@Temperature 20.0 - 300 °C
10.2 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 220 Commercial Bronze, 1/4 Hard
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..
CTE, linear 18.4 µm/m-°C

@Temperature 20.0 - 300 °C
10.2 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 220 Commercial Bronze, 3/4 Hard
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..
CTE, linear 18.4 µm/m-°C

@Temperature 20.0 - 300 °C
10.2 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 220 Commercial Bronze, Annealed
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..
CTE, linear 18.4 µm/m-°C

@Temperature 20.0 - 300 °C
10.2 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 220 Commercial Bronze, Extra Hard
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..
CTE, linear 18.4 µm/m-°C

@Temperature 20.0 - 300 °C
10.2 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 220 Commercial Bronze, Extra Spring
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..
CTE, linear 18.4 µm/m-°C

@Temperature 20.0 - 300 °C
10.2 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 220 Commercial Bronze, Hard
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..
CTE, linear 18.4 µm/m-°C

@Temperature 20.0 - 300 °C
10.2 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 220 Commercial Bronze, Spring
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..
CTE, linear 18.4 µm/m-°C

@Temperature 20.0 - 300 °C
10.2 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 425 Tin Brass 2%, 1/2 Hard
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
CTE, linear 18.4 µm/m-°C

@Temperature 20.0 - 300 °C
10.2 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 425 Tin Brass 2%, 1/4 Hard
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
CTE, linear 18.4 µm/m-°C

@Temperature 20.0 - 300 °C
10.2 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 425 Tin Brass 2%, 3/4 Hard
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
CTE, linear 18.4 µm/m-°C

@Temperature 20.0 - 300 °C
10.2 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 425 Tin Brass 2%, Annealed
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
CTE, linear 18.4 µm/m-°C

@Temperature 20.0 - 300 °C
10.2 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 425 Tin Brass 2%, Extra Hard
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
CTE, linear 18.4 µm/m-°C

@Temperature 20.0 - 300 °C
10.2 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 425 Tin Brass 2%, Extra Spring
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
CTE, linear 18.4 µm/m-°C

@Temperature 20.0 - 300 °C
10.2 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 425 Tin Brass 2%, Hard
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
CTE, linear 18.4 µm/m-°C

@Temperature 20.0 - 300 °C
10.2 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 425 Tin Brass 2%, Spring
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
CTE, linear 18.4 µm/m-°C

@Temperature 21.1 - 871 °C
10.2 µin/in-°F

@Temperature 70.0 - 1600 °F
Carlson C 800 Nickel-Iron-Chromium Alloy
General DescriptionCarlson Alloy C 800 is a nickel-iron-chromium alloy, combining high strength with excellent resistance to oxidation and carburization at elevated temperatures. This alloy resists..
CTE, linear 18.4 µm/m-°C

@Temperature 21.1 - 871 °C
10.2 µin/in-°F

@Temperature 70.0 - 1600 °F
Carlson C 800AT Nickel-Iron-Chromium Alloy
General DescriptionCarlson Alloy C 800AT is a modification of Carlson Alloy C 800, exhibiting higher creep and rupture strengths. This nickel-iron-chromium alloy has a carbon content restricted to ..
CTE, linear 18.4 µm/m-°C

@Temperature 21.1 - 871 °C
10.2 µin/in-°F

@Temperature 70.0 - 1600 °F
Carlson C 800H Nickel-Iron-Chromium Alloy
General DescriptionCarlson Alloy C 800 is a nickel-iron-chromium alloy, combining high strength with excellent resistance to oxidation and carburization at elevated temperatures. This alloy resists..