Thermal Properties Metric English Comments
CTE, linear 18.9 µm/m-°C

@Temperature 20.0 - 649 °C
10.5 µin/in-°F

@Temperature 68.0 - 1200 °F
Eagle Brass 305 Austenitic Stainless Steel, 1/2 Hardened
Type 305 is a chromium nickel stainless steel that can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is nonmagnetic under most conditions. ..
CTE, linear 18.9 µm/m-°C

@Temperature 20.0 - 649 °C
10.5 µin/in-°F

@Temperature 68.0 - 1200 °F
Eagle Brass 305 Austenitic Stainless Steel, 1/4 Hardened
Type 305 is a chromium nickel stainless steel that can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is nonmagnetic under most conditions. ..
CTE, linear 18.9 µm/m-°C

@Temperature 20.0 - 649 °C
10.5 µin/in-°F

@Temperature 68.0 - 1200 °F
Eagle Brass 305 Austenitic Stainless Steel, Annealed
Type 305 is a chromium nickel stainless steel that can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is nonmagnetic under most conditions. ..