Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.01 µm/m-°C @Temperature 23.9 - 260 °C |
2.23 µin/in-°F @Temperature 75.0 - 500 °F |
ASTM E831 |
Saint-Gobain Meldin® 7022 Isostatically Molded Graphite Filled Polyimide Finished parts and basic shapes made from 40% by weight graphite filled polyimide material for applications requiring a low coefficient of thermal expansion, self lubricating properties, and good di.. |