Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 2.50 µm/m-°C @Temperature 23.0 - 260 °C |
1.39 µin/in-°F @Temperature 73.4 - 500 °F |
ASTM D696 |
Daelim H&L Plavis G40 Aromatic Polyimide, 40% Graphite Filled, Direct Formed
(Unverified Data**) Information provided by Daelim H&L |
|||
CTE, linear | 2.50 µm/m-°C @Temperature 20.0 - 100 °C |
1.39 µin/in-°F @Temperature 68.0 - 212 °F |
|
UCAR Carbon UCAR® CBY Extruded Graphite Grade CBY is a general purpose, cost effective extruded graphite with improved strength, structure and density characteristics. It is a low ash graphite for superior oxidation resistance.Typical App.. |
|||
CTE, linear | 2.50 µm/m-°C @Temperature 20.0 - 100 °C |
1.39 µin/in-°F @Temperature 68.0 - 212 °F |
|
UCAR Carbon UCAR® CS Extruded Graphite Densified prior to graphitization, Grade CS is an extruded graphite 25-30% higher in strength than CBY. Grade CS is a low ash graphite with an oxidation resistance similar to grade CBY. It is the ma.. |
|||
CTE, linear | 2.50 µm/m-°C @Temperature 20.0 - 100 °C |
1.39 µin/in-°F @Temperature 68.0 - 212 °F |
|
UCAR Carbon UCAR® CSX Extruded Graphite Densified prior to graphitization, Grade CSX is an extruded graphite, higher in strength and lower in permeability than CS. It is a material for applications requiring higher densities, better mecha.. |
|||
CTE, linear | 2.50 µm/m-°C @Temperature 1000 °C |
1.39 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CRAG-L15 Shroud Nozzle Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 2.50 µm/m-°C | 1.39 µin/in-°F | ASTM E831-93 |
Saint-Gobain Meldin® 1277 Thermoplastic Bearing Material Meldin 1277 has structural integrity and low deformation. This material also exhibits good electrical insulative properties and dimensional stability.Meldin® 1000 series components are used in app.. |