Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 201 µm/m-°C | 112 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® 310M-2 Optically Clear, Flexible Epoxy Material Description: A two component, optically clear, flexible epoxy adhesive designed for optical applications within semiconductor, fiber optic and medical industries. An alternative to EPO-TEK.. |
|||
CTE, linear | 201 µm/m-°C | 112 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® H31 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H31 is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-electronic.. |