Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 23.5 µm/m-°C | 13.1 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1/GF/40/TF/13 Polyamide 66, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
CTE, linear | 23.5 µm/m-°C @Temperature 20.0 °C |
13.1 µin/in-°F @Temperature 68.0 °F |
|
Williams Advanced Alloys WS232 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
CTE, linear | 23.5 µm/m-°C @Temperature 20.0 - 100 °C |
13.1 µin/in-°F @Temperature 68.0 - 212 °F |
|
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |
|||
CTE, linear | 23.5 µm/m-°C @Temperature 20.0 - 100 °C |
13.1 µin/in-°F @Temperature 68.0 - 212 °F |
|
Aleris Hokotol Aluminum Alloy, 200 mm Thickness Sample treatment not specified for property data.Applications include molds for blow forming and injection molding for plastics; bolsters and force plates; high strength/low weight machine parts; an.. |
|||
CTE, linear | 23.5 µm/m-°C @Temperature 20.0 - 100 °C |
13.1 µin/in-°F @Temperature 68.0 - 212 °F |
|
Aleris Hokotol Aluminum Alloy, 100 mm Thickness Sample treatment not specified for property data.Applications include molds for blow forming and injection molding for plastics; bolsters and force plates; high strength/low weight machine parts; an.. |
|||
CTE, linear | 23.5 µm/m-°C @Temperature 20.0 - 100 °C |
13.1 µin/in-°F @Temperature 68.0 - 212 °F |
|
Aleris Hokotol Aluminum Alloy, 300 mm Thickness Sample treatment not specified for property data.Applications include molds for blow forming and injection molding for plastics; bolsters and force plates; high strength/low weight machine parts; an.. |
|||
CTE, linear | 23.5 µm/m-°C @Temperature 20.0 - 100 °C |
13.1 µin/in-°F @Temperature 68.0 - 212 °F |
|
Aleris Hokotol Aluminum Alloy, 325 mm Thickness Sample treatment not specified for property data.Applications include molds for blow forming and injection molding for plastics; bolsters and force plates; high strength/low weight machine parts; an.. |