CTE, linear 248 µm/m-°C
138 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® 730 General Purpose Epoxy
Product Description: EPO-TEK® 730 is a two component, thixotropic, room temperature-curing epoxy adhesive. Advantages & Application Notes: Excellent all purpose adhesive. Many uses in job shop and ..