Thermal Properties Metric English Comments
CTE, linear 486 µm/m-°C

@Temperature 20.0 °C
270 µin/in-°F

@Temperature 68.0 °F
Chlorosulfonated Polyethylene Rubber (CM, CSM)
The chlorine (in CM) or chlorine and chlorosulfonyl (CSM) groups prevent the crystallization that occurs on unmodified polyethylene.