Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 28.1 - 34.8 µm/m-°C @Temperature -60.0 - 60.0 °C |
15.6 - 19.3 µin/in-°F @Temperature -76.0 - 140 °F |
|
Mateck Lithium Fluoride (LiF) Optical crystals |