Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 25.2 - 28.8 µm/m-°C @Temperature 25.0 - 125 °C |
14.0 - 16.0 µin/in-°F @Temperature 77.0 - 257 °F |
|
CMT Materials PROTOBLOCK Air Permeable Prototype Tooling Material PROTOBLOCK is a new composite material made of inorganic granules and epoxy resin engineered to form a micro-porous structure for use as prototype vacuum form or thermoform tooling. The material is.. |
|||
CTE, linear | 21.6 - 28.8 µm/m-°C | 12.0 - 16.0 µin/in-°F | Average value: 24.0 µm/m-°C Grade Count:3 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |