Polymer Property : CTE, linear = 29.9 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 29.9 µm/m-°C
16.6 µin/in-°F
ASTM D696
Ensinger TECATOR™ TI 5013 Polyamide-imide (PAI)
TECATOR™ is a high performance melt processable polyamideimide that maintains its excellent mechanical and wear properties in temperature environments exceeding 500°F. Stock shapes from Ensinger ..