Polymer Property : CTE, linear = 3.17 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 5.70 - 6.10 µm/m-°C

@Temperature 20.0 - 100 °C
3.17 - 3.39 µin/in-°F

@Temperature 68.0 - 212 °F
MarkeTech Cu/Mo/Cu 13:74:13 Laminated Sheet
Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea..
CTE, linear 5.70 µm/m-°C

@Temperature 20.0 - 320 °C
3.17 µin/in-°F

@Temperature 68.0 - 608 °F
Corning Pyroceram® Glass Ceramic
High strength, high elastic modulus, and uniform dielectric properties. Pyroceram® can be manufactured in ogival ( pointed arch) shapes, hemispheres, pressware sheets, and various machined shapes. ..
CTE, linear 5.70 µm/m-°C

@Temperature 1000 °C
3.17 µin/in-°F

@Temperature 1830 °F
Chosun Refractories CH-1 Hard Fireclay brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.70 µm/m-°C

@Temperature 1000 °C
3.17 µin/in-°F

@Temperature 1830 °F
Chosun Refractories N4-1 Fireclay brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.70 µm/m-°C

@Temperature 1000 °C
3.17 µin/in-°F

@Temperature 1830 °F
Chosun Refractories N4-2 Fireclay brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).