Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 5.90 µm/m-°C @Temperature 50.0 - 500 °C |
3.28 µin/in-°F @Temperature 122 - 932 °F |
Pre-fired 1200°C |
Old Hickory No. 1 Glaze Kentucky Ball Clay No. 1 Glaze Clay is a very high kaolin bearing selection with extremely low levels of carbon content. it provides excellent suspension to all types of glazes especially glazes containing a high perc.. |
|||
CTE, linear | 5.90 µm/m-°C @Temperature 20.0 - 1000 °C |
3.28 µin/in-°F @Temperature 68.0 - 1830 °F |
|
McDanel Advanced Ceramics MV-HR1 Mullite Mullite (3Al2O3 • 2SiO2) is a refractory oxide material combining low thermal expansion, good mechanical strength, and resilience at elevated temperatures. Mullite is formulated to produce den.. |