Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 5.94 µm/m-°C @Temperature 20.0 °C |
3.30 µin/in-°F @Temperature 68.0 °F |
|
SGL Carbon Group EK 305 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |