Polymer Property : CTE, linear = 35.7 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 64.3 µm/m-°C
35.7 µin/in-°F
Below Tg
Tra-Con Tra-Bond 216D02 Thixotropic No-Sag Epoxy Adhesive
TRA-BOND 216D02 is a thixotropic, two part epoxy adhesive formulated specifically for applications where a nonsagging adhesive is required. TRA-BOND 216D02 works in concert with TRA-CAST 3135 to per..