Polymer Property : CTE, linear = 36.4 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 36.4 µm/m-°C
20.2 µin/in-°F
BCC Products BC 7136-2 Epoxy Casting
BC7136-2 is an aluminum filled thick section casting system with heat resistance to 300ºF. May be cast to a thickness of 2 inches in non-conductive molds, 3 inches in conductive molds and thicker s..
CTE, linear 36.4 - 40.8 µm/m-°C

@Temperature -60.0 - 60.0 °C
20.2 - 22.7 µin/in-°F

@Temperature -76.0 - 140 °F
Mateck Sodium Chloride (NaCl)
Optical crystals