Polymer Property : CTE, linear = 4.14 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 7.45 µm/m-°C

@Temperature 20.0 °C
4.14 µin/in-°F

@Temperature 68.0 °F
MarkeTech Spinel (MgAl2O4) Single Crystal Substrate
Data provided by the supplier, MarkeTech International.Developed for deposition of III-V nitrides for LEDs, Lasers, etc. Standard orientation: ; GaN Lattice Mismatch 9%.
CTE, linear 7.45 µm/m-°C
4.14 µin/in-°F
at Set Pt.
Ferro IP 550 Thick Film Glass
Glass Type: Pb-Si-B-Al Typical Powder Form: RWG Typical Application: General Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conducto..
CTE, linear 7.45 µm/m-°C
4.14 µin/in-°F
ASTM E831
3D Systems LaserForm™ A6 Tool Steel Powder for Rapid Tooling and Rapid Manufacturing
Parts fabricated from this rapid prototype metal material are actually a blend of stainless steel and bronze. The part is built with steel and subsequently infiltrated with bronze. A6 is great for ..