Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 8.70 µm/m-°C | 4.83 µin/in-°F | |
Plansee MoCu40 Molybdenum-Copper Characteristics:High thermal conductivityLow thermal expansionIdeal for heat dissipation applications related to: IGBT modules, RF packages, and LED chips, among others.Information provided by Plans.. |
|||
CTE, linear | 8.70 µm/m-°C @Temperature 20.0 °C |
4.83 µin/in-°F @Temperature 68.0 °F |
|
Poco Graphite AXF-5QC Specialty Graphite, Copper Impregnated SSH hardness is 67.General Poco Specialty Graphite Information: Poco's high strength, fine-grained, isotropic graphites offer maximum design flexibility. Easily machined. High strength and small p.. |
|||
CTE, linear | 8.70 µm/m-°C @Temperature 260 °C |
4.83 µin/in-°F @Temperature 500 °F |
|
Ferro CF 7555 Low-Temperature Sealing VITREOUS Typical Powder Form: VSD, TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific .. |
|||
CTE, linear | 8.70 µm/m-°C @Temperature 260 °C |
4.83 µin/in-°F @Temperature 500 °F |
|
Ferro CF 1417 Low-Temperature Sealing VITREOUS Typical Powder Form: VSD Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific ther.. |
|||
CTE, linear | 8.70 µm/m-°C @Temperature 20.0 - 300 °C |
4.83 µin/in-°F @Temperature 68.0 - 572 °F |
ISO 7991 |
Schott Glass 8532 Soft Glass Soft glass, free from Na, of high lead content, lower sealing temperature than glass 8531, high dielectric constant Encapsulation of semiconductor components at low temperature (diodes)Information .. |
|||
CTE, linear | 8.70 µm/m-°C @Temperature 20.0 °C |
4.83 µin/in-°F @Temperature 68.0 °F |
|
Goodfellow Iron 77.5/Boron 15/Silicon 7.5 Alloy Metallic glasses (glassy alloys) or amorphous metals. Uses include soft magnetic applications, brazing, coating and as reinforcing fibers.Information provided by Goodfellow. |
|||
CTE, linear | 8.70 µm/m-°C @Temperature 20.0 - 100 °C |
4.83 µin/in-°F @Temperature 68.0 - 212 °F |
|
Goodfellow Platinum 90/Iridium 10 Alloy The alloy has been used in "non-standard" thermocouples, electrical contacts and for electrodes in medical research. The alloy is harder and mechanically stronger than Platinum.Information provided .. |
|||
CTE, linear | 8.69 µm/m-°C @Temperature 0.000 - 300 °C |
4.83 µin/in-°F @Temperature 32.0 - 572 °F |
|
Corning Gorilla® Glass 4 Touch Screen Glass Gorilla® Glass 4 is just as thin and light as previous versions of Gorilla® Glass, but has been formulated to deliver dramatically improved damage resistance allowing improved in-field performance.. |
|||
CTE, linear | 8.70 µm/m-°C | 4.83 µin/in-°F | |
Anderman Ceramics EA95 Sintered Alumina, 95% Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. .. |