Polymer Property : CTE, linear = 423 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 762 µm/m-°C

@Temperature 20.0 °C
423 µin/in-°F

@Temperature 68.0 °F
volumetric
Dow ISONATE™ 125M Pure MDI
ISONATE™ 125M is a crystalline, pure MDI mixture is characterized by high purity, low acidity and reproducible reactivity. This di-functional product is a key ingredient in preparing prepolymers f..
CTE, linear 762 µm/m-°C

@Temperature 20.0 °C
423 µin/in-°F

@Temperature 68.0 °F
volumetric
Dow ISONATE™ 125MDR Pure MDI
ISONATE™ 125MDR is a crystalline, pure MDI mixture is characterized by high purity, low acidity and reproducible reactivity. This difunctional product is a key ingredient in preparing prepolymers ..