Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 87.0 µm/m-°C | 48.3 µin/in-°F | Absolute Drying; ASTM-D696 |
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |