CTE, linear 5.68 µm/m-°C
3.16 µin/in-°F
ac
MarkeTech Calcium Carbonate, Calcite (CaCO3) Optical Grade Crystal
Optical grade crystal with no small inclusions, cleavage planes, clouds and mist, point defects or bubbles inside the crystal. A proprietary process is used for cutting, grinding and polishing quali..