Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.1 - 10.7 µm/m-°C @Temperature 20.0 - 100 °C |
5.61 - 5.94 µin/in-°F @Temperature 68.0 - 212 °F |
|
MarkeTech Mo50Cu Moly/Copper Heat Sink Material MoCu alloys are made by sintering molybdenum and copper together. This results in a heat sink of lower density than tungsten-based materials, low thermal expansion, and excellent thermal conductivit.. |