Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 540 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 540 µm/m-°C

@Temperature 20.0 - 40.0 °C
300 µin/in-°F

@Temperature 68.0 - 104 °F
Solvay Chemicals Polyglycerol-3
A polyglycerol characterized by a very narrow oligomer distribution centered on triglycerol.EINECS Number: 915-741-3/CAS Number: 25618-55-7Information provided by Solvay
CTE, linear 540 µm/m-°C
300 µin/in-°F
Dow Corning FLUOROGEL® 4-8022
One-part, translucent, heat cure, UV indicator, fuel and solvent resistant.Information provided by Dow Corning