Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 40.0 - 56.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
22.2 - 31.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1010 PC (Asia Pacific) |